The sample was thoroughly dried in the solid state to avoid damaging the equipment. Weigh The sample being tested was weighed to 2 mg in a Tzero hermetic aluminum pan. It is best to place the sample directly in the pans, transferring the sample from the weigh paper to the pan can lead to a loss in material. The lid was placed on the pan. It was ensured to place the lid with the indention facing down then the covered pan was placed in the blue holder, assuring that the lid is flush with the top of the holder.

The holder was then placed under the press with lid flushed with the top of the holder. Then the handle was pulled down, thus sealing the pan and lid. Repeat with an empty pan to be used as a reference.

DSC Procedure

The sealed pans were placed in the sample tray, taking note of the slot number and the reference pan was placed in a reference slot also noting the slot number. The reference pan was an empty sealed pan and was used for multiple runs. The power to the cooler was turned on and was ensured to be on event mode.

The software was opened, TA Universal Analysis on the desktop of the computer. In the Control tab, down to event and press the ‘On’ was clicked. This will start the cooler. The ‘Go to standby temp’ was pressed so that the cell does not freeze. The temperature of the cell indicated in the status bar.

Sample volume:
2g
Sample retention:
21 Days
Pickup option:
Both
Operating hours:
Mon 3 - Fri 2

Packaging Instructions

For Liquid samples, per analysis, measure 5ml
Measure 2grams per analysis for solid samples
Liquid samples should be sent in sample bottles, pet bottles, or any air-tight container.
Solid samples should be sent in zip lock bags, sample bottles, or any air-tight container.
Samples should be labeled legibly with paper tape, marker, or writing pen.
Labels should be short and precise (not more than 3 words).
All samples must be strapped together and secured in a bag prior to transport.
Write the Following on the Bag, or Envelope “Allschoolabs Analysis – Receiver: Madison, 08163383206” then add the address of whichever collection center you are sending to.

Comments & Questions (0)

Quick Booking

Book this test, request pickup/drop-off, or ask the lab a question before payment.

Browse More Tests

Related Tests

Tensile Modulus
Allschoolabs · ₦7,000
Dielectric Properties Analysis
Allschoolabs · ₦13,000
Hardness Test
Allschoolabs · ₦4,000
Flexural Modulus
Allschoolabs · ₦7,000